PH23N18
For the production of corrosion products, machine parts, instruments, and the dense porous sheets, ribbons, wires, metallurgical semifinished products (forgings, rods, strips, tubes) and for other purposes.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | High alloy steels and alloys, powder |
Chemical composition
| Standard | Fe, % | Si, % | Ca, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | O, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 13084-88 | 53.89–63 | < 0.1 | < 0.15 | < 0.35 | 21–25 | < 0.08 | 16–20 | < 0.03 | < 0.08 | < 0.02 | < 0.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 13084-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| O | % | Oxygen |