PC-1y
Cobalt powder is intended for the production of powder metallurgy and mgnitov
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Metals and alloys |
Cobalt |
Chemical composition
| Standard |
Fe, % |
Si, % |
Co, % |
Cu, % |
Ni, % |
C, % |
| GOST 9721-79 |
< 0.2 |
< 0.02 |
< 99.35 |
< 0.04 |
< 0.4 |
< 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8900 |
Casting and technological parameters
| melting point, °C |
Boiling temperature, °C |
| 1493 |
2957 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Co |
% |
Cobalt |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| C |
% |
Carbon |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Boiling temperature |
°C |
The boiling point, boiling point is the temperature at which the liquid under constant pressure boils. |