PK10H17N2 (PK10H17N2-6.8, PK10H17N2-7.4)
Scope — product wear and corrosion-resistant (PK10H17N2−6.8); Product dense durable and corrosion-resistant (PK10H17N2−7.4)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Materials of construction |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | C, % |
|---|---|---|---|---|
| GOST 28378-89 | 78.85–83 | 16–18 | 1–3 | < 0.15 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28378-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |