PK10H18N15 (PK10H18N15-6.4, PK10H18N15-6.8, PK10H18N15-7.2, PK10H18N15-7.6)
Scope — Products porous corrosion-resistant (PK10H18N15−6.4, PK10H18N15−6.8, PK10H18N15−7.2); dense products highly corrosive-resistant (PK10H18N15−7.6)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Materials of construction |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | C, % |
|---|---|---|---|---|
| GOST 28378-89 | 64.9–69 | 17–19 | 14–16 | < 0.1 |