PK10H25 (PK10H25-7.4)
Scope — product dense highly corrosive-resistant
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Materials of construction |
Chemical composition
| Standard | Fe, % | Cr, % | C, % |
|---|---|---|---|
| GOST 28378-89 | 73.9–76 | 24–26 | < 0.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28378-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |
| C | % | Carbon |