PK10N4D4 (PK10N4D4-6.4, PK10N4D4-6.8)
Scope — Products srednenagruzhennye porous.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Materials of construction |
Chemical composition
| Standard | Fe, % | Cu, % | Ni, % | C, % |
|---|---|---|---|---|
| GOST 28378-89 | 87.7–96 | 2–6 | 2–6 | < 0.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28378-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cu | % | Copper |
| Ni | % | Nickel |
| C | % | Carbon |