PL1
pig iron for foundry production intended for further processing in the steel or smelting in iron foundries in the production of castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Pig iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | S, % |
|---|---|---|---|---|---|
| GOST 805-95 | 96.95–99.1 | 0.9–1.2 | < 1.5 | < 0.3 | < 0.05 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 805-95 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| S | % | Sulfur |