Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Sb, % |
Al, % |
Pb, % |
Au, % |
Pt, % |
Ir + Rh + Ru, % |
| GOST 13498 - 2010 |
< 0.01 |
< 0.006 |
< 0.005 |
< 0.005 |
< 0.005 |
< 0.006 |
< 0.01 |
> 99.873 |
< 0.08 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
21450 |
111 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| The wire is soft. |
GOST 18389-73 |
0.2–0.5 |
|
|
120–200 |
|
| Wire is hard. |
GOST 18389-73 |
0.2–0.5 |
|
|
350–700 |
|
Casting and technological parameters
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Ir + Rh + Ru |
% |
Iridium + Rhodium + Ruthenium |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| Au |
% |
Gold |
| Pt |
% |
Platinum |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |