Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Sb, % | Al, % | Pb, % | Au, % | Pt, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 34401-18 | < 0.01 | < 0.005 | < 0.005 | < 0.005 | < 0.005 | < 0.005 | < 0.005 | > 99.86 | < 0.1 |
Note: Rh + Rd + Pd + Ir < 0.050