PLA-2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Sb, % | РЗЭ, % | Al, % | Pb, % | Au, % | Pt, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 14837-79 | < 0.01 | < 0.005 | < 0.005 | < 0.005 | < 0.05 | < 0.005 | < 0.005 | < 0.005 | > 99.81 | < 0.1 |
Note: OT: OT + Ag + Mg + Cu + Ni
Note: REM: Pd + Rh + Re + Ir