PLM-2.5 (PLM 97.5)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cu, % | Pt, % | Pd, % | Примеси, % |
|---|---|---|---|---|---|
| GOST 13498-79 | < 0.035 | 2.2–2.8 | 97.2–97.8 | < 0.2 | < 0.23 |
Note: Pd: Pd + Ir + Rh + Au
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 13498-79 | |
| GOST 18389-73 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Cu | % | Copper |
| Pt | % | Platinum |
| Pd | % | Palladium |