Plpd 850-150
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Pb, % | Au, % | Pt, % | Pd, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 18389-14 | < 0.04 | < 0.009 | < 0.015 | < 0.05 | 85–85.5 | 14.276–15 | < 0.11 |
Note: Hallmark: 850
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 24353-14 | |
| GOST 24718-14 | |
| GOST 18389-14 | |
| GOST 30649-99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Pb | % | Lead |
| Au | % | Gold |
| Pt | % | Platinum |
| Pd | % | Palladium |