Plpdrdru81-15-3.5-0.5 (PlPdRdRU-15-3.5-0.5)
For the manufacture of catalytic systems
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Platinum, platinum alloy |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Zn, % |
Pb, % |
Pt, % |
Pd, % |
Rh, % |
Ru, % |
Ir + Au, % |
| GOST 13498 - 2010 |
< 0.03 |
< 0.007 |
< 0.005 |
< 0.01 |
< 0.013 |
79.685–82.2 |
14.5–15.5 |
3.1–3.9 |
0.2–0.8 |
< 0.05 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
18760 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| The wire is soft. |
GOST 13498 - 2010 |
|
|
|
290–390 |
|
Casting and technological parameters
| melting point, °C |
| 1780–1800 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Ir + Au |
% |
Iridium + Gold |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Zn |
% |
Zinc |
| Pb |
% |
Lead |
| Pt |
% |
Platinum |
| Pd |
% |
Palladium |
| Rh |
% |
Rhodium |
| Ru |
% |
Ruthenium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |