Pm
Application: 147Pm isotope is used in phosphors (they glow continuously for several years) and in miniature atomic batteries.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Rare earth metals and their alloys | Promethium |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 7260 |
Casting and technological parameters
| melting point, °C |
|---|
| 1042 |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| melting point | °C | The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |