PMS-K
For the production of sintered products in the automotive, metallurgy, electrical (including return structural shapes), aviation and engineering industries for the manufacture of rings, bushings, bearings, electrical contacts, electrodes, brushes electrical machinery, consumer goods and filters for fine cleaning of oils; The electro industry for sealing contact, for the production of carbon electrodes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Copper Electrolytic Powder |
Chemical composition
| Standard | Fe, % | Cu, % | Sb, % | Pb, % | As, % | O, % |
|---|---|---|---|---|---|---|
| GOST 4960-2009 | < 0.06 | < 99.5 | < 0.005 | < 0.05 | < 0.003 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 4960-2009 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cu | % | Copper |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| O | % | Oxygen |