PMTS36
For soldering brass containing 68% copper
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Copper, copper alloys |
Copper Alloys |
Chemical composition
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
22 |
7700 |
Casting and technological parameters
| melting point, solidus, °C |
melting point, liquidus, °C |
| 800 |
825 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Pb |
% |
Lead |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point, solidus |
°C |
The temperature at which melts the low melting component |
| melting point, liquidus |
°C |
The temperature at which equilibrium falls first crystal |