PNE-2
Electrolytic nickel powder for the manufacture of articles by powder metallurgy, and other purposes. The bulk density of 5.0 g / cm³.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Nickel powder |
Chemical composition
| Standard | Fe, % | Si, % | Co, % | Cu, % | C, % | S, % | O, % | Ni + Co, % |
|---|---|---|---|---|---|---|---|---|
| GOST 9722-97 | < 0.2 | < 0.03 | < 0.5 | < 0.08 | < 0.02 | < 0.01 | < 0.1 | < 99.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 9722-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Co | % | Cobalt |
| Cu | % | Copper |
| C | % | Carbon |
| S | % | Sulfur |
| O | % | Oxygen |
| Ni + Co | % | Nickel + Cobalt |