PNH20K20Y13
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Co, % | Cr, % | Ni, % | Al, % | C, % |
|---|---|---|---|---|---|---|
| < 0.3 | < 20 | < 20 | 46.55–99.99 | < 13 | 0.01–0.15 |
Note: Typical chemical composition
Note: +Y +Si +Nb
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |