PA2
For the production of electro products and other metal-ceramic compositions in various industries
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Tin powder |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Sb, % | Pb, % | As, % | S, % | O, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 9723-73 | < 0.02 | > 99 | < 0.05 | < 0.03 | < 0.05 | < 0.25 | < 0.015 | < 0.016 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 9723-73 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| S | % | Sulfur |
| O | % | Oxygen |