POSSu40-0.5
For tinning and soldering tin, the windings of electrical machines, soldering mounting elements of winding and cable products, radiator pipes, galvanized parts, refrigeration units. Alloy malosurmyanisty recommended for soldering of zinc and galvanized parts
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tin, lead, babity |
Tin-lead solder |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
S, % |
| GOST 21930-76 |
< 0.02 |
39–41 |
< 0.2 |
< 0.05 |
< 0.002 |
< 0.02 |
0.05–0.5 |
< 0.002 |
58.366–60.95 |
< 0.02 |
< 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
9300 |
0.169 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Alloy |
GOST 21930-76 |
|
|
|
40 |
50 |
400 |
|
Brinell hardness number
Casting and technological parameters
| melting point, solidus, °C |
melting point, liquidus, °C |
| 183 |
235 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point, solidus |
°C |
The temperature at which melts the low melting component |
| melting point, liquidus |
°C |
The temperature at which equilibrium falls first crystal |