SUPPORT 36-4
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Sb, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|
| < 0.015 | 58.945–61 | 3.5–4.5 | < 0.015 | < 0.015 | 35.5–36.5 | < 0.01 |