Pr-3V14KB
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Si, % |
Mn, % |
Co, % |
Cr, % |
Sb, % |
P, % |
C, % |
S, % |
W, % |
| TU 5.961-11512-93 |
0.4–1.2 |
0.4–1 |
49.6–58.58 |
26–30 |
0.02–0.1 |
< 0.03 |
2.6–3 |
< 0.07 |
12–15 |