PR-BrA9
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cu, % | Al, % |
|---|---|---|
| > 91 | < 9 |
Note: Typical chemical composition
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cu | % | Copper |
| Al | % | Aluminium |