PR-BrN15Ol8PSR
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Sn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
O, % |
| TU 14-22-33-90 |
< 2 |
0.4–1.2 |
0.1–0.8 |
7–8.5 |
3–4 |
65.72–76 |
13–16 |
0.5–1.2 |
< 0.5 |
< 0.03 |
< 0.05 |