PR-BrO7S10
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Pb, % | P, % |
|---|---|---|---|---|---|---|
| < 0.5 | 7 | 81–82 | 1 | 10 | < 0.5 |
Note: Typical chemical composition
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |
| P | % | Phosphorus |