PR-BrOF8-0.3
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Sn, % | Cu, % | P, % |
|---|---|---|---|
| < 8 | > 91.7 | < 0.3 |
Note: Typical chemical composition
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Sn | % | Tin |
| Cu | % | Copper |
| P | % | Phosphorus |