PR-L63
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cu, % | Zn, % |
|---|---|---|
| > 63 | < 37 |
Note: Typical chemical composition