PRH18N9
Designed for the production of filter elements and a variety of powder metallurgy. The powder is produced from a stainless chromium-nickel steel H18N9 spray air or inert gas.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Stainless chromium-nickel steel and nickel powder |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 14086-68 | 67.025–76 | < 0.8 | < 1 | 16–20 | 8–11 | < 0.035 | < 0.12 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 14086-68 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |