PRV-BrO5TS5S5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Sn, % | Cu, % | Zn, % | Pb, % |
|---|---|---|---|---|
| < 5 | > 85 | < 5 | < 5 |
Note: Typical chemical composition
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |