PSIN 25
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Sb, % |
Pb, % |
As, % |
In, % |
| TU 48-0220-40-90 |
< 0.01 |
< 0.015 |
< 0.01 |
< 0.002 |
< 0.015 |
73.938–76 |
< 0.01 |
24–26 |