PSR 82
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Mg, % | Cu, % | Al, % | Cd, % | Ag, % |
|---|---|---|---|---|---|
| TU 48-1-337-90 | 0.3–0.7 | 2.5–3.3 | 0.3–0.6 | 11.9–16.4 | 79–85 |