PSrKdTSrMg 3
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Mg, % | Zr, % | Cd, % | Ag, % |
|---|---|---|---|---|
| TU 48-1-337-90 | 0.02–0.08 | 0.1–0.3 | 96.12–97.38 | 2.5–3.5 |