PSrLNM 72
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cu, % | Ni, % | Li, % | Ag, % |
|---|---|---|---|---|
| TU 48-1-337-90 | 25.6–27.4 | 0.7–1.3 | 0.4–0.6 | 70.7–73.3 |