PSrMin 63V
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cu, % | Ag, % | In, % |
|---|---|---|---|
| TU 48-1-203-85 | 26–28 | 61.5–64.5 | 9.5–10.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-1-203-85 | |
| TU 48-1-329-89 | |
| TU 48-1-330-89 |