PSrMTSKd 45-15-16-24
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Pb, % |
Cd, % |
Ag, % |
Примеси, % |
| GOST 19738 - 2015 |
< 0.15 |
< 0.005 |
12.045–17.5 |
15–17 |
< 0.15 |
23–25 |
40.045–49.955 |
< 0.15 |
Information on suppliers
Analogues
| Germany |
USA |
| AG 302 |
QQ-B-654 (VII) |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Pb |
% |
Lead |
| Cd |
% |
Cadmium |
| Ag |
% |
Silver |