PSrMTsKd45-15-16-24
Soldering and tinning of non-ferrous metals and steels
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Silver solders |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Pb, % |
Cd, % |
Ag, % |
| GOST 19738-74 |
< 0.15 |
< 0.005 |
12.04–17.35 |
15–17 |
< 0.15 |
23–25 |
44.5–45.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
9400 |
0.065 |
Casting and technological parameters
Analogues
| Germany |
USA |
| AG 302 |
QQ-B-654 (VII) |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Pb |
% |
Lead |
| Cd |
% |
Cadmium |
| Ag |
% |
Silver |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |