PSrOS3-58
Melting point: 180 — 190 ° C
Soldering and tinning of copper, nickel, copper and copper-nickel alloy with silver plated ceramics, soldering silver-plated parts
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Silver solders |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Sb, % |
Pb, % |
Ag, % |
| GOST 19738-74 |
< 0.15 |
55.59–61.31 |
< 0.01 |
0.2–0.8 |
35.89–40.05 |
2.6–3.4 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
8600 |
0.145 |
Casting and technological parameters
| melting point, °C |
| 180–190 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| Ag |
% |
Silver |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |