PSrSu 1-2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Sn, % | Sb, % | Pb, % | Cd, % | Ag, % |
|---|---|---|---|---|---|
| TU 117-1-798-92 | 90.9–93.1 | 1.8–2.2 | 2.7–3.3 | 1.6–2.4 | 0.8–1.2 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 117-1-798-92 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Sn | % | Tin |
| Sb | % | Antimony |
| Pb | % | Lead |
| Cd | % | Cadmium |
| Ag | % | Silver |