PTOM-1
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Si, % | Ti, % | C, % | Cl, % | N, % | H, % |
|---|---|---|---|---|---|---|
| < 0.1 | > 99.366 | < 0.05 | < 0.004 | < 0.08 | < 0.4 |
Note: Typical chemical composition
Note: Fe + Ni <0.40
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Ti | % | Titan |
| C | % | Carbon |
| Cl | % | Chlorine |
| N | % | Nitrogen |
| H | % | Hydrogen |