PV-N55T45
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Fe, % | Ti, % | Ni, % | C, % |
|---|---|---|---|---|
| < 0.2 | 45 | 54.73–55 | < 0.07 |
Note: Typical chemical composition