P3
Applied as an alloying element for production of semiconductor materials, vacuum electrical engineering, in the manufacture of instrumentation, mercury-zinc power sources, chemicals, pharmaceuticals, as well as in the chemical, metallurgical and other industries
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Mercury |
Chemical composition
| Standard | Hg, % |
|---|---|
| GOST 4658-73 | < 99.9 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 4658-73 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Hg | % | Mercury |