R6M5
Steel has an increased tendency to decarburization, increased viscosity, good wear resistance, good grindability.
For all types of cutting tools in the processing of carbon alloyed structural steels; preferably for the manufacture of thread-cutting tools, as well as tools operating with shock loads.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
High speed tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| GOST 19265-73 |
78.395–81.575 |
0.2–0.5 |
0.2–0.5 |
< 0.5 |
3.8–4.4 |
< 0.25 |
< 0.6 |
1.7–2.1 |
< 0.03 |
0.82–0.9 |
< 0.025 |
4.8–5.3 |
5.5–6.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8550 |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Hire |
GOST 19265-73 |
annealing |
255 |
Critical point temperatures
Analogues
| Germany |
USA |
European Union |
| S 6-3-2 |
T11302 |
X80WMoCrV6-5-4 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ar1 |
K |
|