R9F5
For the manufacture of wear-resistant parts.
For the manufacture of simple tools that do not require large volumes of grinding operations in the processing of materials with high abrasive properties; finishing tools simple form in the processing of alloyed steels and alloys.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tool steel |
High speed tool steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| GOST 19265-73 |
76.14–81.5 |
< 0.5 |
< 0.4 |
3.8–4.4 |
< 0.4 |
4.3–5.1 |
< 0.03 |
1.4–1.5 |
< 0.03 |
< 1 |
9–10.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8200 |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Hire |
|
annealing |
269 |
Critical point temperatures
| Ac1, K |
Ac3(Acm), K |
Ar1, K |
| 820 |
850 |
730 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of temperatures of critical points
| Parameter |
Units of measurement |
Description |
| Ac1 |
K |
|
| Ac3(Acm) |
K |
|
| Ar1 |
K |
|