DAM-1
Refined rhodium powder intended for the manufacture of alloys, industrial products and other applications
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Rhodium, rhodium alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Ti, % | Cu, % | Ni, % | Ba, % | Al, % | Pb, % | Ag, % | Au, % | Rh, % | Pt+Pd+Ir+Ru, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 12342-81 | < 0.01 | < 0.005 | < 0.002 | < 0.001 | < 0.005 | < 0.005 | < 0.002 | < 0.005 | < 0.002 | < 0.005 | < 0.003 | < 0.002 | > 99.933 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 12342-81 | |
| GOST 12342-15 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Pt+Pd+Ir+Ru | % | Platinum + Palladium + Iridium + Ruthenium |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Ba | % | Barium |
| Al | % | Aluminium |
| Pb | % | Lead |
| Ag | % | Silver |
| Au | % | Gold |
| Rh | % | Rhodium |