Rua 2
Refined Ruthenium powder for the manufacture of alloys, semi-finished products and other purposes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Ruthenium, Ruthenium Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Ba, % | Al, % | Pb, % | Au, % | Ru, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| GOST 12343-79 | < 0.02 | < 0.01 | < 0.005 | < 0.005 | < 0.01 | < 0.002 | > 99.848 | < 0.1 |