C2C
production of ingots, blocks, ingots for further processing
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | Lead |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Sb, % | Pb, % | As, % | Ag, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 3778-98 | < 0.001 | < 0.001 | < 0.02 | < 0.001 | < 0.001 | < 0.001 | < 99.97 | < 0.001 | < 0.002 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| Germany | USA |
|---|---|
| Pb99.75 | B 29 (Refined Pure Lead) |
Standards
| Standard | Description |
|---|---|
| GOST 3778-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| Ag | % | Silver |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |