САВ1
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Cd, % |
OE, % |
ET, % |
| OST 1 90048-90 |
< 0.2 |
0.7–1.2 |
< 0.00012 |
0.45–0.9 |
< 0.012 |
< 0.012 |
< 0.012 |
< 0.03 |
< 0.03 |
96.87378–98.85 |
< 0.0001 |
< 0.03 |
< 0.7 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Cd |
% |
Cadmium |