Sil1S
For the manufacture of parts of aircraft.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ca, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| OST 1-92014 - 90 | < 0.5 | 10–12.5 | < 0.05 | < 0.1 | < 0.5 | < 0.15 | < 0.02 | < 0.08 | 86.1–90 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1-92014 - 90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |