SK10Mg6
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Si, % | Mg, % | Ca, % | Al, % | P, % |
|---|---|---|---|---|---|
| 76.96–88 | 6–9 | 6–12 | < 2 | < 0.04 |