Precision alloy 30NKF
It is used for the manufacture of parts of high precision instruments requiring dimensional stability in the range of climatic temperatures
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
Soft Magnetic Precision Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Ni, % |
V, % |
ET, % |
| GOST 10994-74 |
48.81–51.6 |
0.1–0.3 |
0.1–0.4 |
18.5–19.5 |
29.5–30.5 |
0.2–0.4 |
< 0.09 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
Cp, Дж/кг·К |
| 20 |
145 |
8400 |
510 |
460 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
d5, % |
Treatment |
| Tape |
TU 14-1-1168-75 |
<2.0 |
Transverse |
|
450–500 |
190–210 |
20–25 |
|
Brinell hardness number
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| Cp |
Дж/кг·К |
Specific heat of material |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |